Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 0.800 kV/mm @Thickness >=3.00 mm |
20.3 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola Etronit IIQ Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Dielectric Strength | 0.800 kV/mm @Thickness >=3.00 mm |
20.3 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Sheets Description: Melamine-based composite material reinforced with glass fabric. High arc resistance and tracking resistance. Flame-resistant. Self-extinguishing.Information provided by Elektro-Isola |