Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.3 kV/mm @Temperature 150 °C |
870 kV/in @Temperature 302 °F |
ASTM D149-97A |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Dielectric Strength | 34.3 kV/mm @Temperature 150 °C |
870 kV/in @Temperature 302 °F |
ASTM D149-97A |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Dielectric Strength | 34.3 kV/mm @Temperature 150 °C |
870 kV/in @Temperature 302 °F |
ASTM D149-97A |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Dielectric Strength | 34.3 kV/mm @Temperature 150 °C |
870 kV/in @Temperature 302 °F |
ASTM D149-97A |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |