Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 29.5 kV/mm @Thickness 1.57 mm |
750 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.57 mm |
750 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP510A Glass Fabric Description: Woven glass fabric epoxy laminate. Engineered to provide NEMA grade FR-4 properties. This material contains bromine on the epoxy resin backbone. Certifiable to MIL-I-24768/27, Type GEE-.. |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.57 mm |
750 kV/in @Thickness 0.0620 in |
Condition - A |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.57 mm |
750 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP680 Paper Base Laminate Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.57 mm |
750 kV/in @Thickness 0.0620 in |
D-48/50 |
Industrial Laminates/Norplex P95 Glass Fabric Description: Woven glass fabric with polyimide resin engineered to maintain excellent physical properties at 240°C. Low coefficient of thermal expansion, high mechanical strength.Thickness Tested.. |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.60 mm |
749 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Valox® 735 PBT 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re.. |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.60 mm |
749 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.60 mm |
749 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 735 PBT+PET 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |