Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 27.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Lexan® 121R PC (Europe-Africa-Middle East)
LEXAN 121R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 121R is available in transparent, translucent and opaque colours.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East)
LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D149
SABIC Innovative Plastics Lexan® IR1840 PC (Europe-Africa-Middle East)
IR1840 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East)
IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D149
SABIC Innovative Plastics Lexan® IR2840 PC (Europe-Africa-Middle East)
IR 2840 resin is a medium-low flow (MFR = 6.5 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Lexan® LI1911R PC (Europe-Africa-Middle East)
Low-viscosity multi-purpose grade having low levels of ionics species.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D149
SABIC Innovative Plastics Lexan® PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics Lexan® PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East)
LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; ASTM D149
SABIC Innovative Plastics Lexan® FL900S PC (Europe-Africa-Middle East)
Foamable Lexan* FL900S polycarbonate resin is an ideal choice for structural components where load bearing capability at elevated temperature is a key requirement. It exhibits outstanding inpact str..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Lexan® ML3982 PC (Europe-Africa-Middle East)
LEXAN ML3982 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D149
SABIC Innovative Plastics PC0703 PC (Asia Pacific)
PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics PC0703 PC (Europe-Africa-Middle East)
PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D 149
SABIC Innovative Plastics PC0703R PC
PC0703R resin is a low flow (MFR = 7 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the extrusion market.This data was supplied by SABIC-IP f..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D149
SABIC Innovative Plastics PC0800 PC (Asia Pacific)
PC0800 resin is a low flow (MFR = 8 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics PC1000 PC (Asia Pacific)
PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D149
SABIC Innovative Plastics PC1000R PC (Asia Pacific)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D 149
SABIC Innovative Plastics PC1800 PC
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D 149
SABIC Innovative Plastics PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D 149
SABIC Innovative Plastics PC1803R PC
PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics PC1803R PC
PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
IEC 60243-1
SABIC Innovative Plastics PC2200R PC (Asia Pacific)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM 2100R PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
ASTM D149
SABIC Innovative Plastics PC1500 PC (Asia Pacific)
PC1500 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Dielectric Strength 27.0 kV/mm

@Thickness 1.60 mm
686 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties
Copyright © lookpolymers.com All Rights Reserved