Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 2.80 kV/mm @Thickness >=3.00 mm |
71.1 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i.. |
|||
Dielectric Strength | 2.80 kV/mm @Thickness >=3.00 mm |
71.1 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Dielectric Strength | 2.80 kV/mm @Thickness >=3.00 mm |
71.1 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Dielectric Strength | 2.80 kV/mm @Thickness >=3.00 mm |
71.1 kV/in @Thickness >=0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Dielectric Strength | 2.80 kV/mm @Thickness 3.17 mm |
71.0 kV/in @Thickness 0.125 in |
100% RH for 96 hours; ASTM D149 |
Garlock BLUE-GARD® 3700 Compressed Aramid Fiber Gasketing, EPDM Binder Aramid fiber, high-temperature fillers, and EPDM binder. For service areas with weak causticsExcellent SealabilityUnique blend of aramid fibers, fillers, and a EPDM rubber binder provides improved t.. |