Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 143R PC (Europe-Africa-Middle East) LEXAN 143R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 143R is available in transparent, translucent and opaque colours. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East) LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 243R PC (Europe-Africa-Middle East) LEXAN 243R is a medium viscosity multi purpose UV stabilized grade and contains release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® GLX143 PC (Europe-Africa-Middle East) Lexan* GLX resin is a medium viscosity grade which is an excellent candidate for applications with high optical quality requirements, such as automotive glazing applications. Available in transparen.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East) LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 143 PC (Europe-Africa-Middle East) LEXAN 143 is a medium viscosity U.V. stabilized multi purpose grade. LEXAN 143 is available in transparent, translucent and opaque colours. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® HP4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2100 PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2100R PEI (Europe-Africa-Middle East) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with .. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Dielectric Strength | 15.0 kV/mm @Frequency 60.0 Hz |
381 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Dielectric Strength | 15.0 kV/mm @Frequency 60.0 Hz |
381 kV/in @Frequency 60.0 Hz |
short time, wet; ASTM D149 |
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 2.00 mm |
381 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 2.0%); ASTM-D149 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.00 mm |
381 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm, Temperature 200 °C |
381 kV/in @Thickness 0.126 in, Temperature 392 °F |
Short Time; ASTM D149 |
DuPont Performance Polymers Rynite® 830ER NC010 PET Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 144 PC (Europe-Africa-Middle East) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |