Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | >= 120 dB | >= 120 dB | @ 1 MHz; Mil Std 285 |
Precision Polymer Engineering S70S Conductive Silicone Rubber Tan coloured, Silicone Rubber, 71-80 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber.Applications: Specially compounded to offer excellent physical and electrical properties.. |
|||
Shielding Effectiveness | 120 dB | 120 dB | @ 10 MHz; Mil Std 285 |
Precision Polymer Engineering S70S Conductive Silicone Rubber Tan coloured, Silicone Rubber, 71-80 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber.Applications: Specially compounded to offer excellent physical and electrical properties.. |
|||
Shielding Effectiveness | >= 120 dB | >= 120 dB | 100 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 120 dB | >= 120 dB | 500 MHz (E Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 120 dB | >= 120 dB | 20 MHz - 10 GHz |
Parker Chomerics CHO-SHIELD® 610 A/B Conductive Epoxy Paint Highly Conductive Epoxy Paint. This is a two-component, silver plated, copper-filled, highly conductive epoxy paint. This coating was developed for application to non-conductive plastic substrates t.. |