Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | >= 115 dB | >= 115 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 115 dB | >= 115 dB | 100 MHz (E Field) - Base/Reinforced Material; MIL-G-83528 |
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |