Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 70 dB | 70 dB | @ 200 kHz; Mil Std 285 |
Precision Polymer Engineering S70L Conductive Silicone Rubber Tan coloured, Silicone Rubber, 66-75 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber. Equivalent to Mil G 83528 Type D.Applications: Specially compounded to offer excellent .. |
|||
Shielding Effectiveness | 70 dB | 70 dB | @ 110 kHz; Mil Std 285 |
Precision Polymer Engineering S70S Conductive Silicone Rubber Tan coloured, Silicone Rubber, 71-80 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber.Applications: Specially compounded to offer excellent physical and electrical properties.. |
|||
Shielding Effectiveness | 70 dB @Frequency 200000 Hz |
70 dB @Frequency 200000 Hz |
Mil std 285 procedure; Mil-G-83528 |
P & P Technology EC-Q(F) Fluorosilicone Elastomer P & P Technology material reference EC-Q(F) is a fluorosilicone elastomer with a Nickel/Graphite conductive filler. Per MIL-G-83528. It is dark green in color. The material is specially compounded t.. |
|||
Shielding Effectiveness | >= 70 dB | >= 70 dB | Chomerics TP08 |
Parker Chomerics CHO-FORM 5532 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553.. |
|||
Shielding Effectiveness | <= 70 dB | <= 70 dB | Modified IEEE-299 |
Parker Chomerics CHOFORM® 5513 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Shielding Effectiveness | >= 70 dB | >= 70 dB | 2 GHz (Plane Wave); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer Conductive Elastomer. CHO-SEAL 1260 elastomer is a silver-filled-silicone intended for mounting silicon wafers during processes such as ion milling. It provides high levels of electrical and thermal.. |
|||
Shielding Effectiveness | >= 70 dB | >= 70 dB | 200 kHz (H Field); MIL-G-83528 |
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 70 dB | >= 70 dB | 50 MHz to 10 GHz; CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 5500 EMI Shielding and Grounding Gasket SOFT-SHIELD 5500 EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electronics, factory automatio.. |
|||
Shielding Effectiveness | 70 dB | 70 dB | ASTM D4935 |
Techmer ES Electrablend® PA6/6 05012 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 2.00e+8 - 1.20e+10 Hz |
>= 70 dB @Frequency 2.00e+8 - 1.20e+10 Hz |
Modified IEEE-299 |
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |