Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 35 - 50 dB @Thickness 3.00 mm |
35 - 50 dB @Thickness 0.118 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX KS002E Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KS002E is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Electrically Conductive, Easy Molding. |
|||
Shielding Effectiveness | 35 dB | 35 dB | ASTM D4935 |
Techmer ES Electrablend® PC/ABS Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc. |