Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 20 dB @Frequency 3.00e+7 - 1.00e+9 Hz |
20 dB @Frequency 3.00e+7 - 1.00e+9 Hz |
ASTM D149 |
Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Shielding Effectiveness | 20 dB @Frequency 3.00e+7 - 1.00e+9 Hz |
20 dB @Frequency 3.00e+7 - 1.00e+9 Hz |
ASTM D149 |
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo.. |
|||
Shielding Effectiveness | 20 - 30 dB | 20 - 30 dB | 1000 MHz; ES7-83 |
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced Carbon Fiber Reinforced |