Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 80 dB @Frequency 1.00e+10 Hz |
80 dB @Frequency 1.00e+10 Hz |
P-Field |
P & P Technology Monel-BS3075 (NA13) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | >= 80 dB @Frequency 1.00e+10 Hz |
>= 80 dB @Frequency 1.00e+10 Hz |
MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1401 Conductive Elastomer High performance for non-corrosive environments; soft(45 Shore A) for low closure force where gasket geometry cannot be exploited; low tear strength; no fluid resistance. Molded and ExtrudedRoHS Com.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 1.00e+8 Hz |
>= 80 dB @Frequency 1.00e+8 Hz |
E-Field; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 5.00e+8 Hz |
>= 80 dB @Frequency 5.00e+8 Hz |
E-Field; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 2.00e+9 Hz |
>= 80 dB @Frequency 2.00e+9 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 1.00e+10 Hz |
>= 80 dB @Frequency 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | 80 dB @Thickness 1.80 mm, Frequency 8.00e+8 - 1.80e+10 Hz |
80 dB @Thickness 0.0709 in, Frequency 8.00e+8 - 1.80e+10 Hz |
IEEE 299 |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+9 Hz |
80 dB @Frequency 1.00e+9 Hz |
1mm x 6mm |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+9 Hz |
80 dB @Frequency 1.00e+9 Hz |
2mm x 6mm |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Shielding Effectiveness | 80 dB @Frequency 100000 Hz |
80 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing... |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+9 Hz |
80 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Teckshield®-F 145 OPI 0.0022" Diameter Wire, High Performance EMC Window Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 1.00e+10 Hz |
>= 80 dB @Frequency 1.00e+10 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1310 Conductive Elastomer Moderate performance in non-corrosive environments, no corrosion or fluid resistance; material of choice for small, delicate injection-molded parts or large dimension extrusionsMolded onlyRoHS Compl.. |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+10 Hz |
80 dB @Frequency 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+10 Hz |
80 dB @Frequency 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+10 Hz |
80 dB @Frequency 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+10 Hz |
80 dB @Frequency 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | >= 80 dB @Frequency 1.00e+8 Hz |
>= 80 dB @Frequency 1.00e+8 Hz |
E-Field; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 80 dB @Frequency 5.00e+8 Hz |
>= 80 dB @Frequency 5.00e+8 Hz |
E-Field; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+8 Hz |
80 dB @Frequency 1.00e+8 Hz |
|
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding.. |
|||
Shielding Effectiveness | 80 dB @Frequency 1.00e+10 Hz |
80 dB @Frequency 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |