Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 102 dB @Frequency 2.00e+9 Hz |
102 dB @Frequency 2.00e+9 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone P & P Technology material reference ECF-J is a fluorosilicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical pro.. |
|||
Shielding Effectiveness | 102 dB @Frequency 2.00e+9 Hz |
102 dB @Frequency 2.00e+9 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-J Silver Aluminum Loaded Silicone P & P Technology material reference EC-J is a silicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.00e+6 Hz |
>= 102 dB @Frequency 1.00e+6 Hz |
H-Field |
P & P Technology Oriented Wires In Silicone P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 4.00e+8 Hz |
>= 102 dB @Frequency 4.00e+8 Hz |
P-Field |
P & P Technology Oriented Wires In Silicone P & P Technology SP, SS, SR, SW & SF Ranges of gasket materials consist of Monel or aluminum wires embedded into solid silicone, sponge silicone or fluorosilicone, a fire retardant variant is also a.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics COMBO® and COMBO® Strip Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel .. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics Frame Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips Clamped in Aluminum ExtrusionsAvailable Forms: Strips, Fab. Lengths, Frames with Joined EMI Strips..Standard Metals Available in EMI Portion: Monel FerrexInf.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics MESH STRIP™ (all metal) Wire Mesh EMI Gasket Selection Guide Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by C.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Woven Wire ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Aluminum OnlyInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics POLASTRIP® Metal EMI Gasket Description: POLASTRIP gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASTRIP gasketing, EMI shieldin.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics PORCUPINE METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Expanded Metal in ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Monel AluminumInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics SHIELDMESH™ Wire Mesh EMI Gasket Selection Guide Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Jointless Rings or Rectangular GasketsStandard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by Ch.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Die-Cut Elastomer with Joined EMI Strips.Standard Metals Available in EMI Portion: Mone.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics MESH STRIP™ (Elastomer Core) Wire Mesh EMI Gasket Selection Guide Construction: Knitted wire mesh over elastomer stripAvailable Forms: Strips, Gaskets Made by Joining Strips, Clip-On Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Informati.. |
|||
Shielding Effectiveness | >= 102 dB @Frequency 1.80e+7 Hz |
>= 102 dB @Frequency 1.80e+7 Hz |
|
Parker Chomerics POLASHEET® Metal EMI Gasket Description: POLASHEET gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASHEET gasketing individual mo.. |