Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 100 dB @Thickness 1.60 mm, Frequency 5.00e+8 Hz |
100 dB @Thickness 0.0630 in, Frequency 5.00e+8 Hz |
MIL G83528 |
Rogers Corporation Bisco® EC-2130 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.063 inches and 0.125 inchesInformation provided by Rogers Corporation. |
|||
Shielding Effectiveness | 100 dB @Frequency 2.00e+9 Hz |
100 dB @Frequency 2.00e+9 Hz |
P-Field |
P & P Technology Conductive Elastomer Nickel Graphite particlesInformation provided by P & P Technology |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+8 Hz |
100 dB @Frequency 1.00e+8 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-H Silver Copper Loaded Fluorosilicone P & P Technology material reference EC-H is a printing grade fluorosilicone elastomer with a Silver/Copper conductive filler and is green in color. The material is specially compounded to offer exc.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+8 Hz |
100 dB @Frequency 1.00e+8 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-H Silver Copper Loaded Silicone P & P Technology material reference EC-H is a printing grade silicone elastomer with a Silver/Copper conductive filler and is Tan in color. The material is specially compounded to offer excellent p.. |
|||
Shielding Effectiveness | 100 dB @Frequency 4.00e+8 Hz |
100 dB @Frequency 4.00e+8 Hz |
P-Field |
P & P Technology Monex Expanded Monel Foil Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+6 Hz |
>= 100 dB @Frequency 1.00e+6 Hz |
E-Field |
P & P Technology Monex Expanded Monel Foil Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
E Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E Field; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and ExtrudedRoHS CompliantInformation provid.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+10 Hz |
>= 100 dB @Frequency 1.00e+10 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E-Field; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
E-Field; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 2.00e+9 Hz |
>= 100 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+10 Hz |
>= 100 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer Extruded onlyInformation provided by Chomerics |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+6 Hz |
100 dB @Frequency 1.00e+6 Hz |
E-Field |
Parker Chomerics WIN-SHIELD® AgF8 Conductive Film Description: Chomerics’ AgF8 conductive film is a multi-layer, silver oxide-based thin film coating applied to a heat stabilized, optical quality polyester film AgF8 film-provides high visible ligh.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+9 Hz |
>= 100 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by .. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+7 Hz |
100 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 100000 Hz |
100 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 100 dB @Frequency 1.00e+7 Hz |
100 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E Field; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 2.00e+9 Hz |
>= 100 dB @Frequency 2.00e+9 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+10 Hz |
>= 100 dB @Frequency 1.00e+10 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer Commercial Grade Conductive Elastomer Extrusions. These materials offer excellent cost/performance characteristics for commercial EMI gasket applications. These silicone and fluorosilicone based con.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 1.00e+8 Hz |
>= 100 dB @Frequency 1.00e+8 Hz |
E Field; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1310 Conductive Elastomer Moderate performance in non-corrosive environments, no corrosion or fluid resistance; material of choice for small, delicate injection-molded parts or large dimension extrusionsMolded onlyRoHS Compl.. |
|||
Shielding Effectiveness | >= 100 dB @Frequency 5.00e+8 Hz |
>= 100 dB @Frequency 5.00e+8 Hz |
E Field; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1310 Conductive Elastomer Moderate performance in non-corrosive environments, no corrosion or fluid resistance; material of choice for small, delicate injection-molded parts or large dimension extrusionsMolded onlyRoHS Compl.. |