Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 0.00 dB @Thickness 0.254 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0100 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.508 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0200 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.813 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0320 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 1.57 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0620 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 2.36 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0930 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 3.17 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.125 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.254 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0100 in, Frequency 8.00e+8 Hz |
NRL Arch Test Method |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.508 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0200 in, Frequency 8.00e+8 Hz |
NRL Arch Test Method |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 3.17 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.125 in, Frequency 8.00e+8 Hz |
NRL Arch Test Method |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 2.36 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0930 in, Frequency 8.00e+8 Hz |
NRL Arch Test Method |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 1.57 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0620 in, Frequency 8.00e+8 Hz |
NRL Arch Test Method |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.813 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0320 in, Frequency 8.00e+8 Hz |
NRL Arch Test Method |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.508 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0200 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 2.36 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0930 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.254 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0100 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 3.17 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.125 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.813 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0320 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 1.57 mm, Frequency 5.00e+8 Hz |
0.00 dB @Thickness 0.0620 in, Frequency 5.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.508 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0200 in, Frequency 8.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 3.17 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.125 in, Frequency 8.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.254 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0100 in, Frequency 8.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 2.36 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0930 in, Frequency 8.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 0.813 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0320 in, Frequency 8.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | 0.00 dB @Thickness 1.57 mm, Frequency 8.00e+8 Hz |
0.00 dB @Thickness 0.0620 in, Frequency 8.00e+8 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |