Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | -1.00 dB @Thickness 0.254 mm, Frequency 5.50e+9 Hz |
-1.00 dB @Thickness 0.0100 in, Frequency 5.50e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -1.00 dB @Thickness 0.508 mm, Frequency 2.80e+9 Hz |
-1.00 dB @Thickness 0.0200 in, Frequency 2.80e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -1.00 dB @Thickness 0.254 mm, Frequency 2.80e+9 Hz |
-1.00 dB @Thickness 0.0100 in, Frequency 2.80e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |