Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 0.500 sec | 0.500 sec | Average value: 0.500 sec Grade Count:4 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 1.77 sec Grade Count:26 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 1.84 sec Grade Count:19 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 0.875 sec Grade Count:4 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 1.81 sec Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS), Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum .. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 1.50 sec Grade Count:9 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 1.00 sec Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 1.50 sec Grade Count:3 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Static Decay | 0.500 - 2.00 sec | 0.500 - 2.00 sec | Average value: 1.50 sec Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |