Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 0.50 sec | 0.50 sec | Charged Plate Monitor; 50% R.H. |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Static Decay | <= 0.50 sec | <= 0.50 sec | 5kV to 50V; FTMS 101C |
Kostat BK-STAT P048BK PP Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |