Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 125 - 135 sec | 125 - 135 sec | ASTM D495 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Arc Resistance | 67.0 - 135 sec | 67.0 - 135 sec | Average value: 107 sec Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Arc Resistance | 130 - 135 sec | 130 - 135 sec | ASTM D495 |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Arc Resistance | 130 - 135 sec | 130 - 135 sec | ASTM D495 |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |