Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 95.0 - 185 sec | 95.0 - 185 sec | Average value: 127 sec Grade Count:6 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |