Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | UL Rating PLC 6 (60-120 sec) |
LG Chemical SG-910 Alphalac Polystyrene
(Unverified Data**) High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliances |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | PLC 6 |
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Arc Resistance | <= 60 sec @Thickness 3.00 mm |
<= 60 sec @Thickness 0.118 in |
UL Rating PLC 7 (<60 sec) |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific) PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics PREVEX VGAX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 180F HDT. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® 553 PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten, PLC code 6; ASTM D 495 |
SABIC Innovative Plastics Noryl HS2000 PPE (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL GFN3L PPE+HIPS (Asia Pacific) PPE+PS, GF30%, hydrolytic stability improved |
|||
Arc Resistance | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL Rating PLC 6 (60-120 sec) |
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa.. |
|||
Arc Resistance | 60 sec | 60 sec | ASTM D495 |
3M Scotch® 70 Self-Fusing Silicone Rubber Electrical Tape Scotch® 24 Brand 70 Silicone Rubber Electrical Tape is a high-temperature arc and track resistance tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner.Informa.. |
|||
Arc Resistance | 60 - 119 sec | 60 - 119 sec | ASTM D495 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
SABIC Innovative Plastics NORYL FN215X PPE+PS Structural foam resin. 170F (77C) HDT. Improved reliability and productivity. All values at 20% weight reduction. |
|||
Arc Resistance | 60 - 119 sec @Thickness 3.00 mm |
60 - 119 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |