Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 134 sec | 134 sec | ASTM D495 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Arc Resistance | 134 sec | 134 sec | ASTM D495 |
Plenco 2369 Phenolic, Granular, Transfer Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Arc Resistance | 134 sec | 134 sec | ASTM D495 |
Plenco 2571 Phenolic, Granular, Compression Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Arc Resistance | 134 sec | 134 sec | ASTM D495 |
Plenco 2408 Phenolic, Granular, Injection Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Arc Resistance | 134 sec | 134 sec | ASTM D495 |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Arc Resistance | 134 sec | 134 sec | ASTM D495 |
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Arc Resistance | 134 sec | 134 sec | ASTM D495 |
Quantum Composites QC-8704FR 63% Glass Fiber Flame Retardant Vinyl Ester SMC
(discontinued **) QC-8704FR is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, an.. |