Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 190 - 195 sec | 190 - 195 sec | ASTM D495 |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |