Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 30.0 - 179 sec | 30.0 - 179 sec | Average value: 116 sec Grade Count:18 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Arc Resistance | 60.0 - 179 sec | 60.0 - 179 sec | Average value: 108 sec Grade Count:20 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D496 |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |
|||
Arc Resistance | 120 - 179 sec @Thickness 3.00 mm |
120 - 179 sec @Thickness 0.118 in |
ASTM D495 |
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas.. |