Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 115 - 125 sec | 115 - 125 sec | ASTM D495 |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Arc Resistance | 110 - 125 sec | 110 - 125 sec | Average value: 120 sec Grade Count:13 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Arc Resistance | 115 - 125 sec | 115 - 125 sec | ASTM D495 |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |
|||
Arc Resistance | 75.0 - 125 sec | 75.0 - 125 sec | Average value: 94.8 sec Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Arc Resistance | 120 - 125 sec | 120 - 125 sec | Average value: 124 sec Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Arc Resistance | 85.0 - 125 sec | 85.0 - 125 sec | Average value: 109 sec Grade Count:8 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |