Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 82.0 - 90.0 sec | 82.0 - 90.0 sec | Average value: 85.8 sec Grade Count:8 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |