Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Plenco 50240 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |
|||
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Plenco 51240 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Arc Resistance | >= 50 sec | >= 50 sec | Test Terminated at 50 sec.; ASTM D495 |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Arc Resistance | >= 50 sec | >= 50 sec | Test Terminated at 50 sec.; ASTM D495 |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Arc Resistance | >= 50 sec | >= 50 sec | ASTM D495 |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Arc Resistance | >= 50 sec | >= 50 sec | ASTM D495 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu.. |
|||
Arc Resistance | >= 50 sec | >= 50 sec | ASTM D495 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
Arc Resistance | >= 50 sec | >= 50 sec | ASTM D495 |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Gharda Chemicals Gafone™ B2315GF Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |
|||
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound
(discontinued **) Polyphenylene Sulfide CompoundRyton® PR09-60 is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments: Test specimen molding con.. |
|||
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound, Annealed 2 hours at 200°C
(discontinued **)&l Polyphenylene Sulfide CompoundRyton® PR09-60 Annealed 2 hours at 200°C is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments.. |
|||
Arc Resistance | 50 sec | 50 sec | ASTM D495 |
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |