Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 125 - 300 sec | 125 - 300 sec | Average value: 190 sec Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-230NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compare.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-230BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compared to oth.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-220BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound formulated for enhanced hydrolytic stability in applications requiring .. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Arc Resistance | 125 sec | 125 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Arc Resistance | 125 sec | 125 sec | Absolute Drying; ASTM-D495 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Arc Resistance | 125 sec | 125 sec | IPC TM-650 2.5.1 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Plenco 7579 Phenolic, Granular, Injection Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
Arc Resistance | 125 sec | 125 sec | ASTM D495 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-200NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low mainten.. |