Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 10 - 18 ohm | 10 - 18 ohm | Coating |
Parker Chomerics Tecknit ECTC™ Windows Electrically Conductive Transparent Coating Description: ECTC WINDOWS are custom designed optical display panels produced by depositing a very thin electrically conductive transparent coating directly onto the surface of various optical subst.. |
|||
Surface Resistivity per Square | 10 - 18 ohm | 10 - 18 ohm | |
Parker Chomerics Tecknit Teckfilm™ Transparent Conductive Coating on Polyester Film Description: TECKFILM is a highly conductive coating deposited on a transparent polyester film. It is available in rolls 30" wide. Usable width is 28". The conductive coating is overcoated with a ce.. |