Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | EOS/ESD S11.11 |
Quadrant EPP Semitron® ESd 520HR (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | EOS/ESD S11.11 |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D648 |
Techmer ES Electrafil® ABS-1200/SD/FR BL ABS |
|||
Surface Resistivity per Square | 1.00e+11 - 1.00e+12 ohm @Temperature 23.0 °C |
1.00e+11 - 1.00e+12 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Surface Resistivity per Square | 1.00e+7 - 1.00e+12 ohm | 1.00e+7 - 1.00e+12 ohm | ASTM D257 |
Ensinger Hydel® PC-P ESD Polycarbonate (PC) HYDEL® PC-P ESD polycarbonate is a static dissipative thermoplastic product containing carbon powder. This material has good stiffness, excellent dimensional ability, and low outgassing properties.. |
|||
Surface Resistivity per Square | 1.00e+9 - 1.00e+12 ohm | 1.00e+9 - 1.00e+12 ohm | ASTM D257 |
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet
(discontinued **) Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical.. |
|||
Surface Resistivity per Square | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | EOS/ESD S11.11 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |