Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.0030 - 0.0090 ohm @Thickness 0.0100 mm |
0.0030 - 0.0090 ohm @Thickness 0.000394 in |
cured |
Gwent Electronic Materials C2121119D9 Nanocopper based Paste This product is a nanocopper based paste that is designed for flat bed screens. The product is compatible with printing on PET substrates such as the DuPont Melinex ST-505. Produced using nano-par.. |