Polymer Property : Surface Resistivity per Square = 150 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 150 ohm
<= 150 ohm
cured; 25 microns thick
Gwent Electronic Materials C2040226D2 Curable Carbon Ink
This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and ..