Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 1.00e+7 - 1.00e+10 ohm | 1.00e+7 - 1.00e+10 ohm | ASTM D257 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-08CF/000 Black Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(disconti Description/Features:Carbon Fiber ReinforcedESD ProtectionPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | VDE 0303 |
GEHR Plastics PE-UHMW-ELS Polyethylene
(discontinued **) Polyethylene offers resistance to almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature of HDPE is from -58 °F to +1.. |
|||
Surface Resistivity per Square | <= 1.00e+7 ohm | <= 1.00e+7 ohm | ASTM D257 |
PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding Information provided by PolyOne™ Corporation |
|||
Surface Resistivity per Square | >= 1.00e+7 ohm | >= 1.00e+7 ohm | VDE 0303 |
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1003 PS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1004 PVC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICS-1005 ABS Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1001 PET Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | after 200% elongation; ASTM D257 |
Kostat ICP-STAT ICD-1004 PVC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | ESD S-11.11-1993 |
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Surface Resistivity per Square | 1.00e+7 - 1.00e+9 ohm @Temperature 23.0 °C |
1.00e+7 - 1.00e+9 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 4211 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Surface Resistivity per Square | 1.00e+7 - 1.20e+8 ohm | 1.00e+7 - 1.20e+8 ohm | |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | |
Bulk Molding Compounds BMC 945 Conductive Grade Bulk Molding Compound BMC 945 is an ESD level Conductive grade of Bulk Molding Compound and is suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reacti.. |
|||
Surface Resistivity per Square | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
PolyOne Edgetek® ES-06CF-09GF/000 GREEN Polyethersulfone - 6% Carbon - 9% Glass Fiber Reinforced - ESD Applications
&am Data provided by PolyOne. |
|||
Surface Resistivity per Square | 1.00e+7 ohm | 1.00e+7 ohm | IEC 60093 |
Arkema Group Pebax® MV 2080 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 2080 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 2080 is an inherently dissipative polymer and can be dry blended or compounded w.. |