Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet) High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PEEK Polyetheretherketone Polyether etherketone can be used at very high temperatures and it shows good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical re.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PEI Polyetherimide Polyetherimide has a high mechanical strength in connection with a good chemical and heat resistance, good dimensional stability and creep resistance. Its unique torque strength permits the economic.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | ASTM D-257 |
Saint-Gobain Norton® FEP Fluoropolymer Film Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | ASTM D-257 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Wanshijie PC Film PC is a kind of shapeless, odorless, non-toxic, high transparency, colorless or light yellow thermoplastic engineering plastic with excellent physical and mechanical properties, especially excellent.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 5 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 8 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 23.0 °C |
1.00e+15 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT™ 2021 Polyimide, Brown (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | ASTM D257 |
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 300 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 48 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PPS Polyphenylene Sulfide The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |