Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
Quadrant EPP PROTEUS® EURO-GRAY Copolymer Polypropylene |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 1250 Crystal Polystyrene
(discontinued **) LACQRENE® 1250 is a very high molecular weight crystal polystyrene mainly for the injection molding industry. It is characterized by a very good compromise between molecular weight, heat resistanc.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | VDE 0303 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm @Temperature 23.0 °C |
1.00e+14 ohm @Temperature 73.4 °F |
50% RH; ASTM D250 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Surface Resistivity per Square | 1.00e+14 ohm @Temperature 23.0 °C |
1.00e+14 ohm @Temperature 73.4 °F |
50% RH; ASTM D250 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D-257 |
Saint-Gobain Norton® PVDF Fluoropolymer Film Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total PSC 1960N Crystal Polystyrene 1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | |
Goodfellow Topas® Cyclo-olefin copolymer Information provided by Goodfellow. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm @Temperature 20.0 °C |
>= 1.00e+14 ohm @Temperature 68.0 °F |
500 V DC at 95% rh; ASTM D257-83 |
DuPont Teijin Films Melinex® 329 Polyester Film, 200 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | Non-adhesive side; ASTM D257 |
3M 4116 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries, PVDF is also gaining rec.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A .. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |