Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 0.075 ohm | <= 0.075 ohm | CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 22.2 °C, Time 1.21e+6 sec |
<= 0.075 ohm @Temperature 72.0 °F, Time 336 hour |
MIL-T-5624 JP-8; CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 71.1 °C, Time 605000 sec |
<= 0.075 ohm @Temperature 160 °F, Time 168 hour |
MIL-H-5606 Hydraulic Fluid; CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 71.1 °C, Time 605000 sec |
<= 0.075 ohm @Temperature 160 °F, Time 168 hour |
MIL-L-7808 Lubrication Oil; CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 85.0 °C, Time 1.21e+6 sec |
<= 0.075 ohm @Temperature 185 °F, Time 336 hour |
CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature -40.0 °C, Time 1.21e+6 sec |
<= 0.075 ohm @Temperature -40.0 °F, Time 336 hour |
CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 85.0 °C, Time 2.59e+6 sec |
<= 0.075 ohm @Temperature 185 °F, Time 720 hour |
CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm | <= 0.075 ohm | CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 22.2 °C, Time 1.21e+6 sec |
<= 0.075 ohm @Temperature 72.0 °F, Time 336 hour |
MIL-T-5624 JP-8; CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 71.1 °C, Time 605000 sec |
<= 0.075 ohm @Temperature 160 °F, Time 168 hour |
MIL-H-5606 Hydraulic Fluid; CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 71.1 °C, Time 605000 sec |
<= 0.075 ohm @Temperature 160 °F, Time 168 hour |
MIL-L-7808 Lubrication Oil; CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 85.0 °C, Time 1.21e+6 sec |
<= 0.075 ohm @Temperature 185 °F, Time 336 hour |
CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature -40.0 °C, Time 1.21e+6 sec |
<= 0.075 ohm @Temperature -40.0 °F, Time 336 hour |
CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Surface Resistivity per Square | <= 0.075 ohm @Temperature 85.0 °C, Time 2.59e+6 sec |
<= 0.075 ohm @Temperature 185 °F, Time 720 hour |
CEPS-0002 |
Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |