Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 0.050 ohm | <= 0.050 ohm | |
Parker Chomerics CHO-SHIELD® 4900 Conductive Coating CHO-SHIELD® 4900 silver-filled acrylic coating provides the highest levels of EMI shielding, as well as anti-static protection and grounding surfaces. It offers convenient fast tack and drying. Fil.. |
|||
Surface Resistivity per Square | <= 0.050 ohm | <= 0.050 ohm | Typically |
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance .. |
|||
Surface Resistivity per Square | <= 0.050 ohm @Thickness 0.0254 mm |
<= 0.050 ohm @Thickness 0.00100 in |
film |
Parker Chomerics CHO-FLEX 601 Conductive Coating CHO-FLEX™ 601 coating is specifically designed for EMI shielding of copper/Kapton flexible circuit laminates and for printing circuits on Kapton film. Upon cure, this coating exhibits excellent adh.. |
|||
Surface Resistivity per Square | <= 0.050 ohm | <= 0.050 ohm | |
Lord Adhesives 6100 Silver Conductor LORD 6100 silver conductor is a one-component, thermosetting conductive epoxy designed primarily for surface mount attachment of electronic component devices. It is recommended for die attach and di.. |
|||
Surface Resistivity per Square | <= 0.050 ohm | <= 0.050 ohm | |
Parker Chomerics CHO-SHIELD® 2052 Conductive Coating CHO-SHIELD® 2052 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Surface Resistivity per Square | <= 0.050 ohm | <= 0.050 ohm | ASTM F390 |
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric P & P Technology material reference NF32B050A21 is a metalised conductive fabric designed for use in EMC shielding and in the manufacture of conductive EMC gaskets. The material is a rip-stop weave .. |