Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 0.0030 ohm | <= 0.0030 ohm | [ohm/in<sup>2<sup>]; <.0005 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FOIL CCE Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Surface Resistivity per Square | <= 0.0030 ohm | <= 0.0030 ohm | [ohm/in<sup>2<sup>]; <.0005 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FOIL CCH Shielding Tape Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti.. |
|||
Surface Resistivity per Square | <= 0.0030 ohm | <= 0.0030 ohm | [ohm/in<sup>2<sup>]; <.0005 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FOIL CCK Shielding Tape Conductive Adhesive Tin-plated Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, alum.. |
|||
Surface Resistivity per Square | <= 0.0030 ohm | <= 0.0030 ohm | |
Lord Adhesives Metech 3255 Silver Conductor This conductor composition is a silver bearing paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The .. |
|||
Surface Resistivity per Square | <= 0.0030 ohm | <= 0.0030 ohm | |
Lord Adhesives Metech 3288 Silver Conductor This product is a silver paste composition designed for screen print application of a solderable electrode base onto various types of electrical ceramic component devices. The fired film forms a hig.. |
|||
Surface Resistivity per Square | 0.0030 - 0.0090 ohm @Thickness 0.0100 mm |
0.0030 - 0.0090 ohm @Thickness 0.000394 in |
cured |
Gwent Electronic Materials C2121119D9 Nanocopper based Paste This product is a nanocopper based paste that is designed for flat bed screens. The product is compatible with printing on PET substrates such as the DuPont Melinex ST-505. Produced using nano-par.. |