Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 4.0 - 10 ohm | 4.0 - 10 ohm | |
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast allycarbonate. A unique feature of Parker Chomerics w.. |
|||
Surface Resistivity per Square | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistivity per Square | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-15NCF/000 ABS - 15% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Surface Resistivity per Square | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D257 |
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Surface Resistivity per Square | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D648 |
Techmer ES Electrafil® J-1200/CF/40 NAT ABS |
|||
Surface Resistivity per Square | 1.0 - 10 ohm | 1.0 - 10 ohm | ASTM D648 |
Techmer ES Electrafil® J-80/CF/20 NAT Acetal (POM) Copolymer |