Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 4.0 - 10 ohm | 4.0 - 10 ohm | |
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast allycarbonate. A unique feature of Parker Chomerics w.. |
|||
Surface Resistivity per Square | 4.0 - 8.0 ohm | 4.0 - 8.0 ohm | printed onto 125µm PET film using 18cm<sup>3</sup>m<sup>-2</sup> anilox |
Gwent Electronic Materials C2110414D7 UV Silver Flexographic Ink UV curable Silver conductor ink specifically designed for printing on to polymeric substrates using flexographic printing. Ink can be printed at speeds up to 13m/min, with good line definition and .. |