Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 150 ohm | <= 150 ohm | cured; 25 microns thick |
Gwent Electronic Materials C2040226D2 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |