Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet) Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 3351(EU) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | VDE 0303 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D-257 |
Saint-Gobain Norton® ETFE Fluoropolymer Film Features/Benefits:Superior release propertiesExcellent weatherabilityPerformance from -200°C (-328°F) to 165°C (330°F)Excellent chemical and mechanical propertiesThermoformableProduct th.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total PSC 1160/1160N Crystal Polystyrene 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. Most notable for the production of bi-oriented polystyrene (BOPS). It is particularly useful.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Surface Resistivity per Square | 1.00e+14 ohm | 1.00e+14 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 32008/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 32008/0009 is an ultra-flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 32008/0009 also has a very low brittleness te.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A .. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0009 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31508/0009 also has a very low brittleness temperatu.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ISO IEC93 |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 31008/0003 Polyvinylidene Fluoride
(discontinued **) 3M™ Dyneon™ PVDF 31008/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31008/0003 also has a very low brittleness temperatu.. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 31008/0009 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesExcellent low flame and low smoke .. |
|||
Surface Resistivity per Square | >= 1.00e+14 ohm | >= 1.00e+14 ohm | < 1V after 2 min - 500 V; ASTM D257 |
3M Dyneon™ PVDF 32008/0000 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesInformation provided by Dyneon, A 3M.. |