Electrical Properties Metric English Comments
Surface Resistivity per Square 0.20 ohm
0.20 ohm
@ 2 mil
Parker Chomerics CHO-SHIELD® 4076-50A Conductive Coating
Conductive Nickel-Filled Coating. This is an electrically conductive waterborne nickel-filled polyurethane coating that provides excellent shielding against radiated EMI. It bonds well to plaster, c..
Surface Resistivity per Square <= 0.20 ohm
<= 0.20 ohm
@ 1 mil
Parker Chomerics CHO-SHIELD® 4925 Conductive Coating
Conductive Coating. CHO-SHIELD 4925 silver and nickel-filled conductive acrylic coating is intended for EMI shielding commercial thermoplastic housings. Its unique solvent system has been formulated..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Surface Resistivity per Square 0.20 ohm

@Thickness 0.0200 mm
0.20 ohm

@Thickness 0.000787 in
Using a 156 stainless steel mesh, 13 micron emulsion
Gwent Electronic Materials C2080409D2 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 85/15. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
cured film; 17 microns thick
Gwent Electronic Materials C60531D1 Silver / Silver Chloride Paste
C60531D1 has a ratio of Silver to Silver Chloride of 90/10. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Ecomass® 1003TU96 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Ecomass® 1003ZD95 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Ecomass® 1005ZD96 Tungsten Powder Filled Co-Polyamide, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Co-Polyamide (COPA), Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing ..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Ecomass® 3608TU96 Tungsten Filled Polyethylene
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyethylene (HDPE)Information provided by Technical Polymers
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Ecomass® 4703TU95 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po..
Surface Resistivity per Square 0.20 ohm
0.20 ohm
ASTM D257
Ecomass® 4703ZD95 Tungsten Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po..
Surface Resistivity per Square 0.20 ohm

@Thickness 0.0250 mm
0.20 ohm

@Thickness 0.000984 in
Normalized, Printed on PET Film
Gwent Electronic Materials C2090210P12 Silver Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..