Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 175 - 500 V | 175 - 500 V | Average value: 308 V Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Comparative Tracking Index | 125 - 500 V | 125 - 500 V | Average value: 273 V Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |