Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 350 V | 350 V | STN EN 60112 |
Plastcom PLASTAMID® 6 GF 30 005 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 30% glass fiber, used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers.. |
|||
Comparative Tracking Index | 350 V | 350 V | STN EN 60112 |
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools.. |
|||
Comparative Tracking Index | 350 V | 350 V | |
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Comparative Tracking Index | >= 350 V | >= 350 V | IEC 60112 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Comparative Tracking Index | 350 V @Temperature 23.0 °C |
350 V @Temperature 73.4 °F |
IEC 60112 |
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Comparative Tracking Index | 350 V | 350 V | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Comparative Tracking Index | 350 V | 350 V | A solution |
LATI Lastilac AR-V0E ABS, Flame Retardant Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av.. |
|||
Comparative Tracking Index | 350 V | 350 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Comparative Tracking Index | 350 V | 350 V | Solution B; IEC 60112 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Comparative Tracking Index | 350 V | 350 V | TS EN 60112 |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC Method |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC Method |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (.. |
|||
Comparative Tracking Index | 350 V | 350 V | Solution A; IEC 60112 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
DSM Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good .. |
|||
Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 350 V | 350 V | M; IEC 60112 |
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 350 V | 350 V | IEC 60112 |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | >= 350 V | >= 350 V | Solution A; IEC 60112 |
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 350 V | 350 V | |
Radici Radiflam® A AE (cond.) Nylon 66 Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Comparative Tracking Index | >= 350 V | >= 350 V | IEC 60112 |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |