Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East) Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by .. |
|||
Comparative Tracking Index | 200 V | 200 V | ASTM D3638 |
Plenco 50030 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
Lanxess Pocan® B 7616 000000 PBT + PC, 15% Glass Fiber PBT+PC, 15% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
SABIC Innovative Plastics Valox® VX8532 PBT+PET (Europe-Africa-Middle East) VALOX VX8532 is a 30% glassfiber reinforced, non blooming, flame retardant PBT+PET blend with excellent surface appearance and good ultrasonic weldability properties.This data was supplied by SABIC-.. |
|||
Comparative Tracking Index | 200 V | 200 V | GB/4207 |
Zhejiang Juner PC-A6-2 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC test |
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac.. |
|||
Comparative Tracking Index | 200 V | 200 V | ASTM D3638 |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Comparative Tracking Index | 200 V @Thickness 3.00 mm |
200 V @Thickness 0.118 in |
IEC 60112; IEC/EN 60893-2 6.4 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Comparative Tracking Index | >= 200 V | >= 200 V | IEC 1212-2 6.4 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Comparative Tracking Index | >= 200 V | >= 200 V | IEC 1212-2 6.4 |
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Comparative Tracking Index | 200 V | 200 V | |
Covestro Bayblend® KL 1-1427 Polycarbonate/ABS Blend Glass fiber reinforced grade (30%) with high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
Comparative Tracking Index | 200 V | 200 V | Solution A; IEC 60112 |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
BASF Ultradur B 4406 G4 Q113 20% Glass Filled PBT Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
DSM Arnite® TV4 264 SN PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Comparative Tracking Index | 200 V | 200 V | GB/4207 |
Zhejiang Juner PC-A1-18 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Comparative Tracking Index | 200 V | 200 V | ASTM D3638 |
Plenco 7552 Phenolic, Nodular, Injection Molded PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re.. |
|||
Comparative Tracking Index | 200 V | 200 V | IEC 60112 |
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |