Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific) 10 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East) Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab.. |
|||
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Lexan® FL403 PC Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"". |
|||
Comparative Tracking Index | 175 V | 175 V | ASTM D3638 |
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded
(discontinued **) This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch.. |
|||
Comparative Tracking Index | 175 V | 175 V | ASTM D3638 |
Plenco Valite 424 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 2424. Data provided by Plenco.VALITE 424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a .. |
|||
Comparative Tracking Index | 175 V | 175 V | Solution A; IEC 60112 |
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR5210R PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_WR5210R compound is a wear resistant, 7% PTFE filled material. |
|||
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
SABIC Innovative Plastics LNP STAT-LOY ZF3021 PPE+PS (Europe-Africa-Middle East) LNP* STAT-LOY* ZF3021 is a compound based on PPE + PS Blend resin containing Glass Fiber. Added features include Antistatic, Flame Retardant. |
|||
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
Teijin Panlite® G-3310M Isotropic, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 10 % of special GF and least anisotropy grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPrecisio.. |
|||
Comparative Tracking Index | 175 - 250 V | 175 - 250 V | PLC code 3; UL 746A |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Comparative Tracking Index | 175 V | 175 V | |
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
Covestro Makrolon® DP1-1888* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-09-3,GF20Developmental productMVR (300 °C/1.2 kg) 10 cm3/10 min20 % Glass fiber reinforcedMilled fiberMedium viscosityEasy releasegood surface qualityInjection molding - Melt te.. |
|||
Comparative Tracking Index | 175 V | 175 V | Solution A; IEC 60112 |
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Comparative Tracking Index | 175 V | 175 V | Solution A; IEC 60112 |
Eurotec® Tecotek® PC44 GR10 GR003 ZG70 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), light grey Information provided by Eurotec® |
|||
Comparative Tracking Index | 175 V | 175 V | ASTM D3638 |
Plenco 7321 Phenolic, Nodular, Injection Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East) LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges. |
|||
Comparative Tracking Index | 175 - 600 V | 175 - 600 V | Average value: 304 V Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |