Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 145 V | 145 V | per 50 drops; ASTM D3638 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Comparative Tracking Index | 145 V | 145 V | IEC test |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |