Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Comparative Tracking Index | 100 - 249 V | 100 - 249 V | Average value: 178 V Grade Count:16 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | Average value: 133 V Grade Count:3 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Comparative Tracking Index | 100 - 250 V | 100 - 250 V | Average value: 160 V Grade Count:13 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati.. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2210 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2212 PEI 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 3452 PEI 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM SILTEM-STM1500 PEI (Europe-Africa-Middle East) SILTEM STM1500 is a flexible siloxane-polyetherimide copolymer for cable and wire coatings. RoHS compliant. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics ULTEM 2110R PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 60112 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Comparative Tracking Index | 100 - 175 V | 100 - 175 V | UL 746A |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Comparative Tracking Index | 100 V @Thickness 3.00 mm |
100 V @Thickness 0.118 in |
IEC 60112; IEC/EN 60893-2 6.4 |
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera.. |
|||
Comparative Tracking Index | 100 V @Thickness 3.00 mm |
100 V @Thickness 0.118 in |
IEC 60112; IEC/EN 60893-2 6.4 |
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets Description: Friction reducing material consisting of phenolic resin and a very fine cotton fabric. Exclusively for mechanical applications. Good dry-run properties but can be lubricated with oil, g.. |
|||
Comparative Tracking Index | >= 100 V | >= 100 V | IEC 1212-2 6.4 |
Hippe PF WV 202 Wood veneer Reinforced Phenolic Resin - Sheet Cross plied. Used in mechanical and electrical applications. Good electrical properties under normal humidity.Information provided by Hippe. |
|||
Comparative Tracking Index | 100 V | 100 V | CTI M; Solution B; IEC 60112 |
Covestro Makroblend® UT5205 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
Comparative Tracking Index | 100 V | 100 V | Test Liquid A; IEC 60112 |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |