Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 22 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 24 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® F 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® FC 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® FC 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® MX 1000 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® MX 1001 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® C CM 406 U Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | IEC Pub1.112, class 2; IEC Method |
Toyobo VYLOPET® EMC407 Non-Reinforced Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessImproved processabilityHigh fluidityGood appearanceInformation provided by Toyobo. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f.. |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.05 mm |
250 - 399 V @Thickness 0.120 in |
UL PLC 2 (250-399 V) |
Resinoid 1312 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Comparative Tracking Index | 250 - 399 V @Thickness 3.00 mm |
250 - 399 V @Thickness 0.118 in |
IEC 60112 |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® 27 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
Comparative Tracking Index | 250 - 399 V | 250 - 399 V | PLC 2; UL 746A |
Mitsubishi Xantar® F 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |